[Functional Introduction]
1. Generally, the test should be carried out at room temperature of 10-35 C.
2. Samples are used to wrap tightly around the mandrel at a prescribed speed not exceeding one circle per second without any torsion. If necessary, the winding speed can be slowed down to prevent the temperature rise from affecting the test results.
3. In order to ensure tight winding, tension force not more than 5% of the corresponding force value of the nominal tensile strength of the wire rod can be applied at the free end of the sample during winding.
4. If unwinding or rewinding after unwinding is required, the speed of unwinding and rewinding should be as slow as possible to prevent temperature rise from affecting the test results. At least one winding ring should be retained at the end of the sample when unwinding.
5. The determination of winding test results shall be carried out in accordance with the relevant standards. If there is no specific requirement, the surface of the sample can be inspected without magnifying tools. If no crack is found, the sample will be qualified. Wire with diameter or thickness less than 0.5mm should be inspected with magnification of about 10 times.
[Technical parameters]
1. Diameter range: 0.5-6 mm
2. Motor parameters: Y80 1-4, 1.5kw 1390r/min
3. Winding speed: 15, 20, 60 r/min
4. Shape size: 700 x 360 x 955 (mm)