1.Twin screw for food extruder Technical specifications
1.Hardness after hardening and tempering: HB280-320
2.Nitrided Hardness: HV850-1000
3.Nitrided case depth: 0.50-0.80mm
4.Nitrided brittleness: less than grade 2
5.Surface roughness: Ra 0.4
6.Screw straightness: 0.015 mm
7.Surface chromium-plating's hardness after nitriding: ≥900HV
8.Chromium-plating depth: 0.025~0.10 mm
9.Alloy Hardness: HRC50-65
10.Alloy depth: 0.8~2.0 mm
2.Features of our 38# CrMoAl screws:
1) High temperature resistance, no deformation under high temperature;
2) Wear resistance, long service life;
3) Corrosion resistance, corrosive materials;
4) High strength, can withstand high torque, high speed;
5) Good cutting performance ;
6) Residual stress after heat treatment is small, thermal deformation is small, and the like.
3.Maintenance precautions
1. Never start the machine when the screw does not reach the preset temperature.
2. Prevent metal fragments and debris from falling into the hopper. If the material is processed and recycled, a magnetic hopper is needed to prevent iron chips from entering the barrel.
3. When using anti-mite, make sure that the plastic in the barrel is completely melted to avoid damage to the transmission system parts when the screw is retracted.
4. When using new plastic, the remaining material of the screw should be cleaned.
5. When the temperature of the molten plastic is normal but it is found that the molten plastic has black spots or discoloration, the rubber snail should be inspected.
6. During processing, try to make the material plasticized evenly, do not let the metal foreign matter mix into the material, and reduce the screw turning torque. force.
Please let me know your demand screw diameter and length,we can make screw according to your require.