Welcome Customer !

Membership

Luoyang Asian Sun Wire & Cable Co., Ltd.
Free Member ·1YRS
,
Other

Main Products: 电线电缆

Xwboo>Products

AAAC Overhead Bare Conductor

Model
Nature of the Manufacturer
Other
Product Category
All Aluminum Alloy Conductor
Place of Origin
City, Province
Overview
Concentric lay stranded Aluminium Alloy Conductors (AAAC) are made out of high strength Aluminium-Magnesium-Silicon Alloy. Our company manufactures and supply AAAC with different variants of electrical grade alloy type 6101 and 6201. one or more strands of hard drawn 1350 aluminium alloy.
Product Details

​All Aluminum Alloy Conductor AAAC Overhead Bare Conductor

Application

AAAC is used as a bare overhead conductor for power transmission and distribution lines, on aerial circuits that require a larger mechanical resistance than AAC, and a better corrosion resistance than ACSR. The sag characteristics and the strength-to-weight ratio of AAAC is better than both AAC / ACSR.

Standards

Basic design to BS 3242 / BS EN 50182 / IEC 61089 / ASTM B 399/B 399M / DIN 48201-6 standards

Cable Construction

AAAC Overhead Bare Conductor  consists of aluminum alloy wires. The aluminum alloy wires are concentrically stranded.

This section deals with heat-treatable magnesium silicon type aluminium alloys to the applicable International Standard, the electrical and mechanical properties of which all fall within the values suggested by relevant standard. Conductors to all other recognized specifications can also be supplied. AAAC Overhead Bare Conductor  he alloysT referred to have higher strength but lower conductivity than pure aluminium. Being lighter, alloy conductors can sometimes be used to advantage in place of the more conventional ACSR; Having lower breaking loads than the later, their use becomes particularly favorable when ice and wind loadings are low.

Electrical Properties

Density@20ºC2.703 kg/dm
Temperature Coefficient@20°C0.00403 (°C)
Resistivity@20°C0.028264
Linear Expansivity23 x10-6 (°C)

Service Conditions

Ambient Temperature-5°C - 50°C
Wind Pressure80 – 130kg/m2
Seismic Acceleration0.12 - 0.05g
Isokeraunic Level10 – 18
Relative Humidity5 – 99%
Density@20ºC2.703 kg/dm
Temperature Coefficient@20°C0.00403 (°C)
Resistivity@20°C0.028264
Linear Expansivity23 x10-6 (°C)